Link to full record for micrograph 82 Micrograph 82 : Aluminium, fracture surface
System: Al, Composition: Not specified
Scanning electron microscopy (SEM)
15 μm
Link to full record for micrograph 83 Micrograph 83 : Aluminium, fracture surface
System: Al, Composition: Not specified
Scanning electron microscopy (SEM)
50 μm
Link to full record for micrograph 604 Micrograph 604 : Extruded aluminium
System: Al, Composition: Commercial purity (99.5%)
Reflected light microscopy, polarised
40 μm
Link to full record for micrograph 605 Micrograph 605 : Fracture surface formed by hot tearing (solidification cracking)
System: Al, Composition: Commercial purity (99.5%)
Scanning electron microscopy (SEM)
40 μm
Link to full record for micrograph 606 Micrograph 606 : Extruded Saffil-containing metal matrix composite
System: Al, Composition: Commercial purity (99.5%)
Reflected light microscopy, polarised
40 μm
Link to full record for micrograph 607 Micrograph 607 : Fibre fracture in a metal matrix composite
System: Al, Composition: Commercial purity (99.5%)
Scanning electron microscopy (SEM)
4 μm
Link to full record for micrograph 608 Micrograph 608 : Channelling contrast TEM image of subgrains of extruded aluminium
System: Al, Composition: Commercial purity (99.5%)
Transmission electron microscopy (TEM)
600 nm
Link to full record for micrograph 609 Micrograph 609 : The grain structure of extruded aluminium
System: Al, Composition: Commercial purity (99.5%)
Reflected light microscopy, polarised
40 μm
Link to full record for micrograph 610 Micrograph 610 : Section of a metal matrix composite (MMC)
System: Al, Composition: Commercial purity (99.5%) + 15 micron angular silicon carbide particles
Reflected light microscopy, polarised
40 μm
Link to full record for micrograph 611 Micrograph 611 : Section of a metal matrix composite (MMC) after extrusion and annealing
System: Al, Composition: Commercial purity (99.5%) + 13 micron alumina spheroids
Reflected light microscopy, polarised
40 μm