3 micrographs for system Cu-Be, ordered by micrograph number.


Link to full record for micrograph 38 Micrograph 38 : Cu 98, Be 2 (wt%), slow cooling - annealing twins
System: Cu-Be, Composition: Cu 98, Be 2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 39 Micrograph 39 : Cu 98, Be 2 (wt%), quenched and aged - annealing twins
System: Cu-Be, Composition: Cu 98, Be 2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 40 Micrograph 40 : Cu 98, Be 2 (wt%), quenched and aged - annealing twins
System: Cu-Be, Composition: Cu 98, Be 2 (wt%)
Reflected light microscopy
80 μm