30 micrographs for technique Cross-polarised light microscopy, ordered by micrograph number.


Showing 1 - 10 of 30 micrographs Page 1 2 3 | Previous | Next

Link to full record for micrograph 156 Micrograph 156 : Roll-bonded aluminium alloy diffusion couple annealed for 30 minutes at 600ºC.
System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%)
Cross-polarised light microscopy
400 μm
Link to full record for micrograph 157 Micrograph 157 : Roll-bonded aluminium alloy diffusion couple annealed for 60 minutes at 600ºC.
System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%)
Cross-polarised light microscopy
750 μm
Link to full record for micrograph 158 Micrograph 158 : Roll-bonded aluminium alloy diffusion couple in the as-rolled condition.
System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%)
Cross-polarised light microscopy
400 μm
Link to full record for micrograph 159 Micrograph 159 : Roll-bonded aluminium alloy diffusion couple in the as-rolled condition.
System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%)
Cross-polarised light microscopy
2 mm
Link to full record for micrograph 566 Micrograph 566 : Inversion wall revealed by spontaneous band texture in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1)
Cross-polarised light microscopy
50 μm
Link to full record for micrograph 567 Micrograph 567 : Wedge disclinations revealed by spontaneous band texture in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1)
Cross-polarised light microscopy
50 μm
Link to full record for micrograph 568 Micrograph 568 : Strain induced birefringence in a thermoformed PET cup
System: Polyethylene terephthalate (PET), Composition: Not specified
Cross-polarised light microscopy
8 mm
Link to full record for micrograph 569 Micrograph 569 : Injection-moulded polystyrene ruler
System: Polystyrene (PS), Composition: Not specified
Cross-polarised light microscopy
11 mm
Link to full record for micrograph 570 Micrograph 570 : Strain-induced birefringence in a notched polycarbonate bar
System: Polycarbonate (PC), Composition: Not specified
Cross-polarised light microscopy
6 mm
Link to full record for micrograph 571 Micrograph 571 : Strain-induced birefringence in a polycarbonate bar
System: Polycarbonate (PC), Composition: Not specified
Cross-polarised light microscopy
14 mm