Technique
30 micrographs for technique Cross-polarised light microscopy, ordered by micrograph number.
Showing 1 - 10 of 30 micrographs | Page 1 2 3 | Previous | Next |
Micrograph
156
:
Roll-bonded aluminium alloy diffusion couple annealed for 30 minutes at 600ºC. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 400 μm |
|
Micrograph
157
:
Roll-bonded aluminium alloy diffusion couple annealed for 60 minutes at 600ºC. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 750 μm |
|
Micrograph
158
:
Roll-bonded aluminium alloy diffusion couple in the as-rolled condition. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 400 μm |
|
Micrograph
159
:
Roll-bonded aluminium alloy diffusion couple in the as-rolled condition. System: Al-Fe-Mn/Al-Si, Composition: Al, Fe 0.5, Mn 1.0 / Al, Si 1.0 (wt%) Cross-polarised light microscopy 2 mm |
|
Micrograph
566
:
Inversion wall revealed by spontaneous band texture in a liquid crystalline polymer System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1) Cross-polarised light microscopy 50 μm |
|
Micrograph
567
:
Wedge disclinations revealed by spontaneous band texture in a liquid crystalline polymer System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1) Cross-polarised light microscopy 50 μm |
|
Micrograph
568
:
Strain induced birefringence in a thermoformed PET cup System: Polyethylene terephthalate (PET), Composition: Not specified Cross-polarised light microscopy 8 mm |
|
Micrograph
569
:
Injection-moulded polystyrene ruler System: Polystyrene (PS), Composition: Not specified Cross-polarised light microscopy 11 mm |
|
Micrograph
570
:
Strain-induced birefringence in a notched polycarbonate bar System: Polycarbonate (PC), Composition: Not specified Cross-polarised light microscopy 6 mm |
|
Micrograph
571
:
Strain-induced birefringence in a polycarbonate bar System: Polycarbonate (PC), Composition: Not specified Cross-polarised light microscopy 14 mm |
Showing 1 - 10 of 30 micrographs | Page 1 2 3 | Previous | Next |