Image Link to full record for video 73 video 73 : Fan blade containment test in a Rolls Royce turbine engine. One blade in a turbine engine is released using a charge. The blade must be contained within the engine to consider it safe for use.
Image Link to full record for video 74 video 74 : The first Tacoma Narrows (Puget Sound, near the city of Tacoma, Washington) suspension bridge collapsed due to wind-induced vibrations (7-11-1940).
Image Link to full record for video 156 video 156 : Coarse particles in Water (Viscosity ~ 10-3 Pa s) - μ ~ 30 mm s-1
Image Link to full record for video 157 video 157 : Fine particles in Water (Viscosity ~ 10-3 Pa s) - μ ~ 1 mm s-1
Image Link to full record for video 158 video 158 : Coarse particles in Oil (Viscosity ~ 5 10-2 Pa s) - μ ~ 0.5 mm s-1
Image Link to full record for video 159 video 159 : Fine particles in Oil (Viscosity ~ 5 10-2 Pa s) - μ ~ 0.02 mm s-1
Image Link to full record for video 160 video 160 : Laser Scattering with 30 ?m particles in suspension
Image Link to full record for video 161 video 161 : Laser Scattering with 200 ?m particles in suspension
Image Link to full record for video 165 video 165 : Dislocations (Frank Reid source)
Image Link to full record for video 167 video 167 : Foam being compressed in a cell