Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

DoITPoMS Video Library Full Record for Video 69

Full Record for Video 69

Click to view video 69
[10 sec, audio: No]

View video in new window

Download
Windows media file [783 Kb]
Quicktime video [1206 Kb]
video no
69
Brief description
Video of the movement of a dislocation in a ferritic steel at elevated temperature, taken in a TEM.
Categories
TEM
Date
10/08/06
Licence for re-use
DoITPoMS standard terms of use