Full Record for Video 91
[8 sec, audio: No]
View video in new window
Download
Windows media file [976 Kb]
Quicktime video [5049 Kb]
- video no
- 91
- Brief description
- Melt Spinning or "Splat quenching" to produce metallic glass ribbon. Molten tin alloy is fed through several nozzles onto a rotating metal drum, resulting in extremely high cooling rates (approx. 1 million Kelvin per second). High speed photography at 4000 fps. From the TLP Casting
- Categories
- Experimental procedure
- Date
- 06/09/06
- Licence for re-use
- DoITPoMS standard terms of use