Categories > Foam > Polyurethane (PU) > X-ray tomography > Keyword: polymer composite foam

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 581 Micrograph 581 : X-ray tomography image of open cell polyurethane foam
System: Polyurethane (PU), Composition: Not specified
X-ray tomography
1.5 mm