Micrograph no
866
Brief description
Low Carbon Steel
Keywords
Categories
Metal or alloy
System
Fe-C-X   Link to phase diagram
Composition
Fe, C 0.9 (wt%)
Standard codes
Reaction
Processing
Applications
Sample preparation
Technique
Atomic force microscopy (AFM)
Length bar
5 μm
Further information
An AFM of fine pearlite. Platelets are revealed as they rotate orientation throughout the sample area.
Contributor
Rachel Oliver
Organisation
Department of Materials Science and Metallurgy, University of Cambridge
Date
12/08/10
Licence for re-use
Attribution-NonCommercial-ShareAlike 4.0 International