AimsBefore you startIntroductionDislocation generationDislocation interactions Sessile dislocationsClimb and cross slipDislocation intersections to form jogs and kinksDeformation of a single crystalForest hardeningContinuum models describing the true stress-strain curvesGrain boundary hardening of poly-crystalsSummaryQuestionsGoing furtherTLP creditsTLP contentsShow all contentViewing and downloading resourcesAbout the TLPsTerms of useFeedbackCredits Print this page
PreviousNext
Before you start
This TLP assumes that you have some basic knowledge on dislocation theory. However, the following TLPs could be helpful:
Introduction to Dislocations (Basic information about dislocations)
Slip in Single Crystals (Information about slip in an fcc metal, including stage I and II of its deformation)