Image | video 83 : A three-point bend test to measure the deflection and failure load of a wet balsa sample. From TLP The Structure and Mechanical Behaviour of Wood |
Image | video 84 : Shows disassembly of a cheap lighter to determine its components. From the TLP Examination of a Manufactured Article |
Image | video 90 : Melt Spinning or "Splat quenching" to produce metallic glass ribbon. Molten tin alloy is fed through a nozzle onto a rotating metal drum, resulting in extremely high cooling rates (approx. 1 million Kelvin per second). High speed photography at 4000 fps. |
Image | video 91 : Melt Spinning or "Splat quenching" to produce metallic glass ribbon. Molten tin alloy is fed through several nozzles onto a rotating metal drum, resulting in extremely high cooling rates (approx. 1 million Kelvin per second). High speed photography at 4000 fps. From the TLP Casting |
Image | video 97 : The construction of a KNO3 capacitor, and the hysteresis loop it displays. The circuit used is the standard Sawyer-Tower circuit. From TLP Ferroelectric materials |
Image | video 98 : When a magnet is brought near a spinning disk it causes magnetic flux changes and the formation of eddy currents, which consist of moving charges and hence are themselves magnetic fields. Repulsive forces between the 2 magnetic fields cause the spin of the disk to slow. From TLP Recycling of metals |
Image | video 129 : Showing how driving a wedge into layers of plastacine piles up the material displaced from the indent onto the surface. |
Image | video 133 : The sample moves though θ (~5 to 45 °) while the detector scans though 2θ (~10 to 90 ° ). It has been speeded up as typical data collection time would be somewhere between 10 mins and 10 hours. From the TLP X-ray Diffraction Techniques |
Image | video 135 : The shape memory effect as demonstrated by the Ferris wheel. The wheel is made up of 10 springs stretched apart by weights. The video shows what happens when the springs are heated. From the TLP Superelasticity and Shape Memory Alloys |
Image | video 136 : The shape memory effect: close up of the cooling of the springs in a Ferris wheel. From the TLP Superelasticity and Shape Memory Alloys |